SNAA427 October   2025 HDC1010 , HDC1080 , HDC2010 , HDC2021 , HDC2022 , HDC2080 , HDC3020 , HDC3020-Q1 , HDC3021 , HDC3021-Q1 , HDC3022 , HDC3022-Q1 , HDC3120 , HDC3120-Q1

 

  1.   1
  2.   Abstract
  3.   Trademarks
  4. 1Introduction: Why RH Sensors Appear Out-of-Spec
    1. 1.1 Where and When do RH Errors Occur?
    2. 1.2 What are the Root Causes of RH Errors?
    3. 1.3 Case Studies
  5. 2Definitions: Key Terms for RH Accuracy
  6. 3Initial Troubleshooting Steps
    1. 3.1 Initial Verification Steps
    2. 3.2 Diagnostic Questions
  7. 4Common Sources of RH Error - Prevention and Mitigation
    1. 4.1 PCB and Enclosure Design Considerations
      1. 4.1.1 PCB Thermal Transfer to RH Sensor
      2. 4.1.2 Power Supply Noise and Analog RH Sensors
      3. 4.1.3 Enclosure Design & Airflow Considerations
    2. 4.2 Assembly, Soldering, and Manufacturing Processes
      1. 4.2.1 Assembly Instructions: What to Avoid
      2. 4.2.2 Assembly Instructions: Best Practices
      3. 4.2.3 Sensor Cavity Protection During Assembly
    3. 4.3 Rehydration Post-Assembly
      1. 4.3.1 Recovering Sensor Accuracy Post-Soldering
      2. 4.3.2 Rehydration Procedure
    4. 4.4 Test Setup and Environment
      1. 4.4.1 RH References
      2. 4.4.2 Setup Uniformity: Controlled Environment
      3. 4.4.3 Setup Uniformity: Thermal Gradients
      4. 4.4.4 Settling Time
    5. 4.5 Storage and Handling
      1. 4.5.1 Storage Temperature and Humidity Conditions
      2. 4.5.2 Storage Materials
      3. 4.5.3 How Does MSL Level Relate to RH Sensors?
      4. 4.5.4 Handling Best Practices
    6. 4.6 Chemical Contamination
      1. 4.6.1 How Chemical Contamination Affects RH Accuracy
      2. 4.6.2 Where and How are Chemical Contaminants Introduced?
      3. 4.6.3 Mitigating Effects of Chemical Contamination: Bake
      4. 4.6.4 Mitigating Effects of Chemical Contamination: Cleaning
      5. 4.6.5 Mitigating Effects of Chemical Contamination: Enclosure Design
      6. 4.6.6 Mitigating Effects of Chemical Contamination: Device Selection
      7. 4.6.7 Mitigating Effects of Chemical Contamination: Assembly Considerations
    7. 4.7 Operating Conditions: Application Environment Conditions and Effects
      1. 4.7.1 Environmental Conditions That Contribute to RH Accuracy Errors
      2. 4.7.2 RH Offset Mitigation & System-Level Design
      3. 4.7.3 Using the Integrated Heater
    8. 4.8 RH Accuracy Debugging Flowchart
  8. 5Summary: Designing for and Debugging RH Accuracy
  9. 6References
  10. 7Appendix
    1. 7.1 Case Study 1: Humidity-Induced Positive RH Offset
    2. 7.2 Case Study 2: Gradual RH Accuracy Drift in 100%RH Environment
    3. 7.3 Case Study 3: Combined Factors from Assembly & Thermal Effects

Definitions: Key Terms for RH Accuracy

This section defines key terms for discussing RH accuracy. Understanding the concepts presented in this section is critical to being able to evaluate, diagnose, prevent, and mitigate RH accuracy errors with the methods presented in Section 4 of this document.

  • Sensing Polymer: capacitive-based RH sensors utilize an exposed polymer to capture moisture in the air. This captured moisture fills voids in the polymer, which alters the dielectric constant of the polymer. This change in dielectric constant creates a change in capacitance for the sensing electrode beneath the polymer. Temperature and humidity conditions can also affect how the polymer senses humid air, along with other unwanted components such as other chemicals. Figure 2-1 shows a simplified sensor structure, with the polymer acting as the media which captures moisture from the air.
 Sensing Polymer ExampleFigure 2-1 Sensing Polymer Example
  • RH Error: the difference between the RH sensor’s humidity measurement and a calibrated reference.
  • RH Hysteresis: the difference between the up curve (RH error as ambient RH increases) or down curve (RH error as ambient RH decreases) and the centered average of the up and down curves. Positive RH hysteresis is the gap between the centered average and the down curve, negative RH hysteresis is the gap between the centered average and the up curve. Hysteresis occurs because the sensing polymer has a memory of the humidity conditions this has seen before. Hence the RH sensor's RH error will be slightly negative when previously exposed to low RH conditions, and slightly positive when previously exposed to high RH conditions. The exact shape of the RH hysteresis can change with different ambient temperatures. Figure 2-2 shows two different views of the "up & down" curves, one for RH error vs reference RH ,and the other shows measured RH vs reference RH.
 RH Hysteresis ExampleFigure 2-2 RH Hysteresis Example
 RH Offset Error ExampleFigure 2-3 RH Offset Error Example
  • RH Offset: refers to a positive or negative shift in RH error that is constant over different ambient RH levels and temperatures. Figure 2-3 demonstrates how %RH error can flatly increase across RH levels.
  • RH Gain: refers to a shift in RH error that is not constant over humidity; for example, a positive RH gain may have low RH error at low humidity and a high RH error at high humidity, while a negative RH gain may have high RH error at low humidity and low RH error at high humidity. Figure 2-4 shows two examples of RH gain. On the left is an example of negative RH gain, and on the right an example of positive RH gain. Note how at low RH levels the effects of gain shift can be minimal, but as RH increases the effects become more pronounced. In many real-world cases, RH offset and RH gain can be combined.
     RH Gain Error ExampleFigure 2-4 RH Gain Error Example
  • VOCs: Volatile Organic Compounds. VOCs are organic chemicals, often human-made, that have a high tendency to vaporize into the air, otherwise known as "off-gassing". VOCs can negatively impact RH accuracy by interfering with the normal operation of the sensing polymer. Because VOCs can vaporize into the air at ambient conditions, they are a common source of chemical contamination for polymer based humidity sensors.
  • MSDS: material safety data sheet. The MSDS for a given product (for example, a particular conformal coating, shipping foam, solder paste, and so on) can detail most if not all of the chemicals in the product. Obtaining and reading the MSDS is key to avoiding potential chemical contaminants, so that user's can choose products that minimize impact to RH accuracy.
  • SEM: Scanning electron microscopy. Used to take high resolution images of sensing polymer, can be useful in identifying deposited chemical contaminants
  • EDX: Energy dispersive X-ray spectroscopy. A failure analysis technique that shows the chemical composition through spectroscopy of a spot on the sensing polymer. Very useful to determine the nature of a chemical contaminant. This is considered destructive failure analysis because of the thin layer of metal deposition required, so no further RH testing can be done on a unit that undergoes EDX.